Yes. however make sure you leave the tanking slurry to dry for at least 7 days before applying plaster boards.
No Hydro Tanking Slurry
How long does it take for tanking slurry to dry?
Curing procedures should be strictly adhered to. It is important that the surface of the slurry is protected from strong sunlight and drying winds, with either a suitable curing compound, polythene sheeting, damp hessian or similar, for a minimum of 48 hours. If Tanking Slurry will be left unprotected, fine mist spray the surface 3 […]
Does tanking slurry work?
Yes, tanking slurry waterproofs against positive and negative hydrostatic heads of water and is suitable for use, internally, externally, above and below ground.
How thick should tanking slurry be?
Tanking slurry is a minimum 2 coat application, with each layer applied at a uniform thickness of at least 1 mm per coat.
What is tanking slurry?
Tanking slurry is a cementitious waterproofing system which creates a monolithic bond using crystalline chemicals when applied to concrete and masonry structures.